Anhui Hechuang New Synthetic Materials Co., Ltd

Anhui Hechuang New Synthetic Materials Co., Ltd

Manufacturer from China
Verified Supplier
3 Years
Home / Products / HDPE Geomembrane Sheet /

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining

Contact Now
Anhui Hechuang New Synthetic Materials Co., Ltd
Visit Website
City:hefei
Province/State:anhui
Country/Region:china
Contact Person:Xu
Contact Now

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining

Ask Latest Price
Video Channel
Brand Name :Geomax
Model Number :Geomembrane
Certification :CE
Place of Origin :ANHUI CHINA
MOQ :1000 Square Meter
Price :Negotiation
Payment Terms :T/T, L/C
Supply Ability :10000suqre Mater/Day
Delivery Time :7 -20days
Packaging Details :Packed in The Woven Bags orCcustomized
Material :HDPE LDPE LLDPE PVC PE
Length :50-200m
Width :1m~8m
Thickness :0.2mm~3mm
Transport Package :HDPE Geomembrane Liner Is Packed in The Woven Bags
Specification :0.5mm 0.75mm 1.0mm 1.5mm 2mm
Origin :Anhui, China
Application :Transportation Project, Hydraulic Project, Geotechnical Project, Environmental Project
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

PRODUCT DESCRIPTION

Smooth Textured HDPE LDPE LLDPE PVC Geomembrane For Dam Pond Liner Landfill Mining

Product Introduction

Construction Method
1. The slope shall be laid in order from top to bottom. Don't pull it too tight.
2. Tow adjacent longitudinal joints should not be in a horizontal line, should bestaggered more than 1m each other.
3. Longitudinal joints should be more than 1.50m away from the dam foot and bending foot, and should be located on the plane.
4. When the slope is laid, the direction of spreading film should be basically parallel to the slope line.
5. The construction, first of all to use small diameter sand or clay levelingbase, and then laid the geomembrane. The geomembrane should not be stretched too tight, and the part of the soil bured at both ends is corrugated. A transitional layer of about 10cm is laid on the geomembrane with sand or clay.

Specifications

Specification Test method Unit Type
thickness ASTM 05199 mm 0.75 1 1.25 1.5 2
density ASTM 0 1505 g/cm3. min. 0.939 0.939 0.939 0.939 0.939
tensile strength at yield ASTM 06693 KN/m. min. 11 15 18 22 29
tensile strength at break ASTM 06693 KN/m. min. 20 27 33 40 53
elongation at yield ASTM 06693 %.max. 12 12 12 12 12
elongation at break ASTM 06693 %.max. 700 700 700 700 700
tear resistance ASTM 0 1004 N 93 125 156 187 249
puncture resistance ASTM 04833 N 240 320 400 480 640
environment stress cracking resistance ASTM 05397 hr 300 300 300 300 300
carbon black content ASTM 0 1603 % 2-3 2-3 2-3 2-3 2-3
oxidation induction time (OIT) ASTM 03895 minute 100 100 100 100 100
low temperature
(-70'C)impact brittle
ASTM 02136 pass pass pass pass pass
stream hydraulic conductivity g.cm/(cm².s.Pa),
max.
1x10¯13 1x10¯13 1x10¯13 1x10¯13 1x10¯13
dimension stability after 2 storge 1 h/100'C ASTM 0 1204 %.max 2 2 2 2 2

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining


HCNS Manufacture

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining

Exhibition 30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining

Our Certificates and HDPE Geocell Testing reports

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining

Inquiry Cart 0